Content
- 1 1. Why LSZH Cable Insulation Matters in Construction Engineering
- 2 2. Product Overview and Application Concept
- 3 3. Rapid LED UV Cross-Linking Technology
- 4 4. Fire Performance for Class B1 and B2 Applications
- 5 5. Halogen-Free, Low-Corrosiveness Design
- 6 6. Mechanical and Electrical Performance
- 7 7. Thermal Resistance and Cross-Linked Structure
- 8 8. Representative Technical Data
- 9 9. Advantages Compared with Conventional Cable Compound Options
- 10 10. Manufacturing Strengths and Technical Infrastructure
- 11 11. Quality Control from Formulation to Finished Compound
- 12 12. Processing Guidance for Cable Manufacturers
- 13 13. Potential Applications
- 14 14. Sustainability and Energy-Saving Benefits
- 15 15. Product Selection and Qualification Considerations
- 16 16. Frequently Asked Questions
- 16.1 What is UV Irradiation Cross-linked LSZH Insulation?
- 16.2 How quickly does the material cure?
- 16.3 What are the main benefits compared with traditional irradiation cross-linking?
- 16.4 Are the B1 and B2 grades suitable for construction cables?
- 16.5 Does the product contain halogens?
- 16.6 What smoke-density results are reported?
- 16.7 What mechanical properties are available?
- 16.8 Does the material resist heat deformation?
- 16.9 Can the compound be used on existing extrusion lines?
- 16.10 What quality support does the manufacturer provide?
- 16.11 How should customers choose between the listed grades?
- 17 17. Conclusion
- 18 References
- 19 Product: UV Irradiation Cross-linked LSZH Flame Retardant Insulation for Construction Engineering (Class B1/B2)




UV Irradiation Cross-linked LSZH Flame Retardant Insulation for Construction Engineering (Class B1/B2)
Low-smoke, zero-halogen cable materials are increasingly important in buildings, transportation facilities, public infrastructure, data centers, power distribution systems, and other locations where fire safety and occupant protection are critical. In these applications, cable insulation must perform several functions at the same time. It must provide reliable electrical insulation, withstand mechanical stress during manufacturing and installation, resist thermal deformation, restrict flame spread, limit smoke generation, and avoid the release of corrosive halogen-containing gases during combustion.
UV Irradiation Cross-linked LSZH Flame Retardant Insulation for Construction Engineering, available in Class B1 and Class B2 grades, is designed to address these combined requirements. The material uses a UV curing process after extrusion. Exposure to LED ultraviolet light initiates cross-linking within only a few seconds, allowing the extrusion and curing stages to operate in a highly coordinated production sequence. Compared with traditional irradiation cross-linking, this method can substantially shorten curing time, reduce equipment requirements, lower energy consumption, and improve production efficiency.
The product is classified within the UV Crosslinked LSZH Compound category. Its formulation is intended for cable insulation used in construction engineering and related safety-sensitive applications. The Class B1 and B2 versions are developed to meet the combustion performance requirements described in GB 31247-2014, including flame propagation, heat release, total heat release, smoke density, burning drips, combustion particulates, toxicity of combustion gases, and corrosiveness.
Beyond its fire-performance profile, the material offers a balanced combination of tensile strength, elongation, electrical insulation, heat resistance, low acidity, and low conductivity. This balance is essential because a flame-retardant compound must not sacrifice processability or cable reliability simply to achieve a lower fire risk. The product is therefore positioned as an application-oriented solution for manufacturers that need efficient production together with dependable cable performance.
1. Why LSZH Cable Insulation Matters in Construction Engineering
Cables installed in buildings are often routed through enclosed or difficult-to-evacuate spaces. These spaces may include corridors, shafts, ceiling voids, electrical rooms, communication rooms, tunnels, transportation stations, hospitals, schools, commercial buildings, and residential developments. During a fire, the cable jacket or insulation can influence how quickly flames travel, how much smoke is produced, and whether corrosive or toxic gases are released.
Conventional halogen-containing cable materials can generate acidic gases and dense smoke when exposed to fire. Acidic gases may corrode metal equipment, damage electronic systems, and create additional hazards for emergency responders. Dense smoke can obscure exit routes and reduce visibility. The use of low-smoke, zero-halogen materials is therefore a major strategy for improving fire safety in occupied and infrastructure-intensive environments.
LSZH compounds are designed to reduce halogen-related risks. The term “low smoke, zero halogen” generally refers to materials that do not rely on halogen-containing polymers as the principal insulation or sheathing system and that are formulated to limit smoke and corrosive gas generation. For construction applications, however, the LSZH designation alone is not enough. The compound must also satisfy mechanical, electrical, thermal, processing, and fire-performance requirements appropriate to the final cable design.
UV cross-linking adds another important dimension. Cross-linking changes the polymer structure from a primarily melt-processable system into a network with improved resistance to heat, deformation, and environmental stress. When the cross-linking reaction is completed rapidly after extrusion, cable manufacturers can obtain the performance benefits of a cross-linked insulation system without relying on long curing cycles or large conventional irradiation facilities.
2. Product Overview and Application Concept
UV Irradiation Cross-linked LSZH Flame Retardant Insulation is extruded onto a conductor and then cured by exposure to LED UV light. The light activates the material’s cross-linking system, allowing the insulation to develop its intended network structure within seconds. This process is especially attractive for high-throughput cable manufacturing because the curing stage can be integrated closely with extrusion.
The product is offered in standard and fire-performance-oriented grades, including DS-ZWG-105, DS-ZWG-125, DS-ZWG-105-B1, and DS-ZWG-105-B2. The grade names indicate product variants intended for different temperature or fire-performance requirements. Final cable design, conductor size, extrusion conditions, wall thickness, color, and installation environment should be evaluated before selecting a grade.
The Class B1 and Class B2 materials are aimed at construction engineering cables where flame behavior and smoke control are especially important. The products are designed to address the combustion performance requirements of GB 31247-2014. These requirements extend beyond a simple vertical flame test. They consider several aspects of fire behavior, such as the way a flame propagates, how much heat is released, whether burning droplets occur, the amount of smoke produced, and the characteristics of gases and particulates generated during combustion.
In practical terms, the material is intended for cable manufacturers that need a compound suitable for modern building safety systems while also seeking a streamlined production process. It can be considered for power cables, control cables, communication cables, building wiring, and other cable constructions where an LSZH cross-linked insulation is appropriate. The exact suitability depends on the cable standard, conductor design, voltage rating, installation conditions, and required certification pathway.
3. Rapid LED UV Cross-Linking Technology
The most distinctive processing feature of this material is its rapid LED UV curing system. After the compound is extruded, the insulation passes through a controlled UV exposure zone. The energy from the LED UV source activates the cross-linking reaction. According to the supplied product information, the process takes only a few seconds and can be dozens of times faster than traditional irradiation cross-linking.
Traditional cross-linking methods may require significant equipment, extended residence time, or separate production stages. A long curing process can increase the length of the production line, raise energy consumption, complicate line balancing, and reduce manufacturing flexibility. The rapid UV approach is intended to overcome these limitations by placing the curing stage close to the extrusion process.
The ability to combine extrusion and cross-linking offers several operational benefits. First, it can reduce production cycle time. A shorter cycle may help manufacturers improve line output without adding a proportionate amount of floor space. Second, it can lower the investment required for large conventional irradiation equipment. Third, it may reduce energy use because LED UV systems can deliver curing energy efficiently and operate only when production is underway. Fourth, a compact curing arrangement can support more flexible plant layouts.
Rapid curing also supports process consistency when the UV dose, line speed, material temperature, and cooling conditions are controlled properly. In a modern cable plant, the process can be monitored through parameters such as extrusion pressure, melt temperature, line speed, UV intensity, exposure distance, exposure time, insulation diameter, and spark-test performance. These controls help manufacturers maintain a stable cross-linking level from one production run to the next.
Although the curing stage is fast, successful production still depends on proper process design. The cable producer must match the material grade with the extruder, screw configuration, die design, cooling system, and UV equipment. The UV source must provide suitable intensity and uniformity across the cable surface. The line should also prevent contamination, uncontrolled cooling, or excessive surface damage before curing is complete. The compound supplier’s technical support is therefore an important part of achieving reliable industrial performance.
3.1 Comparison with Traditional Irradiation Cross-Linking
Traditional irradiation cross-linking normally uses high-energy radiation equipment to modify the polymer after extrusion. Such equipment may require a substantial capital investment, dedicated shielding arrangements, specialized operating controls, and careful radiation-safety management. The process can be technically effective, but its scale and operating requirements may not be suitable for every cable manufacturer.
UV cross-linking uses LED ultraviolet light as the activation source. Its potential advantages include a compact system, lower energy demand, rapid activation, and easier integration into an extrusion line. The process is particularly attractive where the manufacturer wants to add a cross-linked LSZH product without building a large radiation-processing facility.
The comparison should be understood as a process advantage rather than a universal replacement claim. The optimum technology depends on the polymer formulation, cable construction, production speed, required cross-linking level, and customer specification. Nevertheless, the rapid UV approach gives manufacturers an additional option for producing high-performance LSZH insulation with a shorter and potentially more economical production route.
4. Fire Performance for Class B1 and B2 Applications
Fire performance is the central application value of this product. The Class B1 and Class B2 grades are designed for construction engineering requirements identified in GB 31247-2014. The supplied description states that the products address flame propagation, heat release rate, total heat release, smoke density, burning drips, combustion particulates, toxicity of combustion gases, and extremely low corrosiveness.
These criteria are important because fire behavior is multidimensional. A cable that stops burning quickly may still release substantial heat or produce heavy smoke. A material with limited flame spread may still create burning droplets that ignite nearby materials. Similarly, low smoke volume alone does not fully describe the hazard if the combustion gases are highly corrosive. A comprehensive fire-performance approach considers the complete behavior of the material under the specified test conditions.
The B1 and B2 designations provide manufacturers with options for different construction requirements. In general, a higher fire-performance classification is selected when the building design, local regulations, cable installation method, or project specification demands stronger control of flame spread and heat release. The final classification of a cable assembly should be confirmed through testing of the finished cable, because conductor type, insulation thickness, fillers, screens, tapes, bedding, sheath construction, and installation configuration can all influence fire behavior.
The product data also reports low smoke density values. For flame conditions, the typical values listed for DS-ZWG-105, DS-ZWG-125, DS-ZWG-105-B1, and DS-ZWG-105-B2 are 50, 50, 45, and 40, respectively, against a stated limit of 100. Under non-flame conditions, the typical values are 300, 305, 255, and 265, against a stated limit of 350. These figures indicate that the supplied grades are formulated to limit smoke generation under the listed test conditions.
Smoke reduction has direct practical value in buildings. Lower smoke density can help preserve visibility, support evacuation, and reduce the difficulty of locating the source of a fire. It may also reduce contamination of sensitive spaces and equipment. However, smoke behavior depends on the complete cable construction and the actual fire scenario, so laboratory values should be used as part of a broader product qualification program.
5. Halogen-Free, Low-Corrosiveness Design
The product’s LSZH profile is supported by the listed HCl and HBr content, pH value, and conductivity data. The typical HCl and HBr content for all four listed grades is below 0.5 percent, matching the stated maximum requirement. The pH values range from 5.0 to 5.2, compared with a stated minimum of 4.3. Conductivity values range from 0.51 to 0.53 microsiemens per millimeter, compared with a stated maximum of 10.
These measurements are significant because acidic combustion products can damage metal components and electronic equipment. A low level of hydrogen chloride and hydrogen bromide is consistent with the objective of a low-corrosiveness, halogen-free cable system. The pH result provides an indication of the acidity of combustion products in the relevant test solution, while conductivity can help characterize the ionic content of the combustion gases or condensate under the specified test method.
In a building filled with electrical systems, the secondary damage caused by corrosive smoke can be severe. Even after the visible fire is controlled, acidic deposits may affect switchgear, sensors, control panels, communication equipment, and data-processing systems. LSZH materials are therefore valuable not only for protecting people but also for reducing damage to infrastructure and shortening recovery time after a fire event.
The low-corrosiveness design is also relevant to transport and industrial applications. Rail systems, ships, power stations, renewable-energy facilities, and communication centers often contain densely packed cables and expensive electronic equipment. A compound that limits smoke and acidic gases can support a more comprehensive fire-safety strategy across these environments.
6. Mechanical and Electrical Performance
Fire performance must be balanced with mechanical integrity. During extrusion, cabling, transport, installation, and service, insulation may experience pulling, bending, compression, abrasion, thermal cycling, and contact with other materials. The supplied performance data show that the product family combines flame-retardant characteristics with tensile strength and elongation values suitable for cable insulation development.
The stated minimum tensile strength is 10.0 MPa. The typical tensile strengths are 12.5 MPa for DS-ZWG-105, 13 MPa for DS-ZWG-125, 11 MPa for DS-ZWG-105-B1, and 11.5 MPa for DS-ZWG-105-B2. The typical elongation at break values are 170 percent, 175 percent, 160 percent, and 165 percent, respectively, compared with a stated minimum of 150 percent.
These values indicate a useful combination of strength and flexibility. Tensile strength helps the insulation withstand handling and installation forces, while elongation at break provides a margin against cracking or rupture when the cable is bent or pulled. The precise mechanical behavior of the finished cable will also depend on insulation thickness, conductor stranding, extrusion conditions, and any additional layers surrounding the insulation.
Electrical insulation performance is another fundamental requirement. The listed volume resistivity at 20 degrees Celsius ranges from 4.5 times 10 to the power of 14 to 5.8 times 10 to the power of 14 ohm-centimeters. The stated standard value is 1.0 times 10 to the power of 14 ohm-centimeters. The dielectric strength values are 28 or 30 megavolts per meter, against a stated minimum of 20 megavolts per meter.
High volume resistivity helps limit leakage current through the insulation. Dielectric strength indicates the material’s ability to withstand an electric field without electrical breakdown under the specified test conditions. Together, these properties support the use of the compound in cable insulation designs where stable electrical separation is required.
Manufacturers should still validate electrical performance on the finished cable. Conductor geometry, insulation eccentricity, moisture exposure, voids, surface defects, and processing contamination can influence the final result. A high-quality compound is an important foundation, but precise extrusion and in-line quality control remain essential.
7. Thermal Resistance and Cross-Linked Structure
Cross-linking is valuable because it improves the dimensional and thermal stability of polymer insulation. When a cable operates at elevated temperature or experiences a temporary overload, an adequately cross-linked material can resist deformation more effectively than an equivalent uncross-linked material. This helps preserve insulation thickness and electrical reliability.
The product data include elongation-under-load and heat-elongation results. The listed elongation under load shows tensile strength change rates of approximately +10 to +15 percent under the specified conditions, with maximum elongation change rates from -12 to -17 percent after 168 hours. These figures are presented within a stated change-rate requirement of plus or minus 25 percent.
For heat elongation at 200 degrees Celsius under a 0.2 MPa load for 15 minutes, the listed elongation under load values are 45 percent, 40 percent, 35 percent, and 40 percent for the four grades. The stated maximum is 100 percent. Permanent deformation after cooling is listed as zero for all four grades against a stated maximum of 25 percent.
These results suggest that the cross-linked insulation maintains good dimensional stability at elevated temperature and returns effectively after the specified heat-load test. Low permanent deformation is especially important because excessive deformation can reduce insulation thickness, change electrical clearances, and increase the possibility of failure in service.
The supplied table contains some compressed or nonstandard formatting in the descriptions of the heat-aging conditions. Cable manufacturers should therefore confirm the exact test method, specimen conditioning, temperature, time, load, and acceptance criteria with the technical data sheet and laboratory documentation before using the values for formal qualification.
8. Representative Technical Data
The following table reorganizes the supplied typical values for convenient comparison. The values are representative data and should be verified against the current technical data sheet, purchase specification, and applicable test report before being used for design approval.
| Test Item | Unit | Requirement or Standard | DS-ZWG-105 | DS-ZWG-125 | DS-ZWG-105-B1 | DS-ZWG-105-B2 |
|---|---|---|---|---|---|---|
| Specific gravity | g/cm³ | Reference value | 1.49 | 1.48 | 1.58 | 1.57 |
| Tensile strength | MPa | ≥10.0 | 12.5 | 13.0 | 11.0 | 11.5 |
| Elongation at break | % | ≥150 | 170 | 175 | 160 | 165 |
| Volume resistivity at 20°C | Ω·cm | 1.0 × 1014 | 5.8 × 1014 | 5.6 × 1014 | 4.5 × 1014 | 5.0 × 1014 |
| Dielectric strength | MV/m | ≥20 | 30 | 30 | 28 | 28 |
| Smoke density under flame | — | ≤100 | 50 | 50 | 45 | 40 |
| Smoke density without flame | — | ≤350 | 300 | 305 | 255 | 265 |
| pH value | — | ≥4.3 | 5.0 | 5.0 | 5.2 | 5.1 |
| HCl and HBr content | % | ≤0.5 | <0.5 | <0.5 | <0.5 | <0.5 |
| Conductivity | μS/mm | ≤10 | 0.52 | 0.53 | 0.51 | 0.52 |
| Impact catalytic temperature | °C | -25 | Pass | Pass | Pass | Pass |
The data show that all four grades meet or exceed the stated values for the listed mechanical and electrical tests. The B1 and B2 variants also show lower typical smoke density under flame than the two general grades in the supplied comparison. Grade selection should be based on the required fire class, operating temperature, cable construction, extrusion conditions, and project specification rather than on one property alone.
9. Advantages Compared with Conventional Cable Compound Options
The product’s competitive advantages arise from the combination of material performance and manufacturing efficiency. Many cable compounds may provide one or two desirable characteristics, but construction cables require a wider set of properties. The UV cross-linked LSZH system is designed to combine low smoke, halogen-free combustion behavior, mechanical strength, electrical insulation, thermal stability, and fast processing.
Compared with conventional thermoplastic LSZH insulation, a cross-linked material can provide improved resistance to heat deformation and permanent set. This can be important in cables exposed to elevated operating temperatures or short-duration thermal stress. The cross-linked network also supports dimensional stability during heat-related testing.
Compared with traditional irradiation-cross-linked materials, the LED UV process can reduce curing time and simplify the required equipment configuration. The supplied information states that the curing speed is dozens of times faster than traditional irradiation cross-linking. This can help manufacturers increase output, reduce energy use, and lower the equipment investment associated with the curing stage.
Compared with halogen-containing insulation, the LSZH formulation is intended to reduce corrosive gas generation and smoke hazards. This is particularly valuable in occupied buildings and areas containing sensitive electrical and electronic equipment. The reported pH, HCl and HBr, and conductivity results support the product’s low-corrosiveness objective.
Compared with a material optimized only for flame retardancy, the product offers a broader performance balance. Tensile strength, elongation, dielectric strength, volume resistivity, heat elongation, and permanent deformation are all included in the supplied data. This broader profile helps cable manufacturers evaluate the compound as a complete insulation solution rather than as a single-purpose additive system.
Competitor comparisons should always be based on equivalent test methods and complete cable assemblies. Fire classifications, smoke results, and mechanical properties can vary significantly depending on specimen preparation and cable design. The strongest comparison is therefore a controlled evaluation using the same conductor, insulation thickness, extrusion line, conditioning procedure, and laboratory method.
10. Manufacturing Strengths and Technical Infrastructure
Jiangsu Duoshang New Materials Technology Co., Ltd. is located in Nantong, Jiangsu Province, China, and specializes in the research, development, production, and sales of polyolefin cable compounds. The company’s manufacturing and technical resources support its ability to develop application-specific materials for power, communications, locomotives, photovoltaics, new energy generation, rail transit, marine cables, and other industries.
The company operates a research and development center of more than 3,000 square meters. The center is equipped with more than RMB 35 million worth of research equipment and supported by a professional team of more than 30 research and development personnel, including five doctors and several recipients of provincial and municipal talent awards. This structure provides a foundation for formulation development, process optimization, performance testing, and customer-specific technical support.
Duoshang also operates two production bases covering more than 15,000 square meters, with more than 10 production lines for polyolefin cable compounds. The production network includes UV-cross-linked compounds, silane cross-linkable compounds, irradiation cross-linked compounds, thermoplastic LSZH flame-retardant compounds, polyethylene sheath compounds, and other specialized materials.
This breadth is important because cable manufacturers do not always need a single material. A project may require an insulation compound, a sheath compound, a communication-cable material, a photovoltaic cable solution, or a material compatible with a specific extrusion line. A supplier with experience across multiple polyolefin technologies can better understand how different layers interact in a complete cable structure.
The company’s stated philosophy combines people-oriented management with technology-driven innovation. Its product development approach emphasizes application-oriented solutions, research and testing support, technical documentation, stable supply capability, and customized material solutions for customers worldwide. These capabilities are particularly relevant for UV cross-linked LSZH products, where successful implementation depends on both formulation quality and process integration.
11. Quality Control from Formulation to Finished Compound
Quality control begins with raw-material selection. LSZH formulations commonly require a careful balance of polymer matrix, flame-retardant system, smoke-suppressing components, stabilizers, processing aids, cross-linking ingredients, pigments, and other functional additives. Each component must be selected for compatibility, dispersion, thermal stability, and effect on electrical insulation.
Compounding conditions are equally important. Mixing temperature, residence time, shear rate, feeding accuracy, and pelletizing conditions influence additive dispersion and batch uniformity. Poor dispersion can cause surface defects, weak points, unstable color, variations in flame performance, or reduced electrical reliability. Consistent production requires controlled dosing and a reproducible mixing profile.
After compounding, manufacturers may assess appearance, pellet dimensions, moisture, density, melt behavior, tensile properties, elongation, volume resistivity, dielectric strength, smoke density, acidity, conductivity, and thermal deformation. Production batches should be traceable through raw-material records, equipment settings, test results, packaging information, and shipment documentation.
For customers, technical documentation is an important part of quality assurance. A useful documentation package may include a technical data sheet, safety information, processing guidance, recommended extrusion conditions, batch certificate, test report, and storage recommendations. Where a project requires formal compliance, the customer should request the relevant certification and confirm whether the certificate applies to the compound, the finished cable, or a specific cable construction.
12. Processing Guidance for Cable Manufacturers
Before production, the compound should be stored in a clean, dry area and protected from moisture, dust, direct sunlight, and excessive heat. Packaging should remain sealed until the material is ready for use. If the technical data sheet specifies pre-drying or conditioning, the manufacturer should follow that procedure. Moisture and contamination can affect surface quality, electrical properties, and UV curing behavior.
The extrusion line should be selected or configured for the viscosity and thermal sensitivity of the material. Important variables include screw design, compression ratio, barrel temperature profile, head temperature, die geometry, conductor preheating, line speed, cooling-water temperature, and take-up tension. Stable melt pressure and uniform insulation diameter are essential for reliable cable quality.
UV curing requires additional controls. LED wavelength, optical intensity, exposure distance, exposure time, and surface coverage should be matched to the material system. The UV source must be maintained so that intensity does not fall below the qualified process window. Line speed should be controlled together with UV dose rather than adjusted independently. If the cable passes too quickly through the UV zone, the cross-linking level may be insufficient; if the process is unnecessarily slow, productivity may be reduced.
After curing, the cable may be checked through hot-set or heat-elongation testing, gel-content or cross-linking evaluation where applicable, dimensional inspection, spark testing, tensile testing, and electrical testing. Process qualification should include start-up, steady-state, line-speed changes, color changes, and planned shutdown conditions. These evaluations help determine whether the material remains stable across normal manufacturing variations.
The exact processing window should be developed jointly with the supplier. Because cable designs differ, a condition that works for a small communication cable may not be suitable for a large power cable. The conductor diameter, insulation wall thickness, pigment package, extrusion throughput, and UV equipment all affect curing performance.
13. Potential Applications
The product is primarily associated with construction engineering cables. These may include building power cables, control cables, instrumentation cables, communication cables, alarm cables, and other low-smoke cable systems used in indoor or enclosed environments. The material can also be considered for infrastructure projects where cable fire behavior is a major design concern.
Data centers are one potential application area. These facilities contain large quantities of power and communication cables, as well as high-value electronic equipment. Low smoke and low corrosiveness can help reduce the secondary impact of a fire, while cross-linked insulation supports the thermal and electrical requirements of continuous operation.
Transportation facilities, including rail stations, tunnels, airports, and other public facilities, may also benefit from LSZH cable systems. Such environments often have large numbers of occupants, limited evacuation routes, and extensive cable networks. The combination of flame-retardant performance and smoke control can support the overall fire-safety strategy of the facility.
Hospitals, schools, commercial complexes, and high-rise buildings are additional application areas. In these buildings, cable routes may pass through multiple fire compartments or serve critical systems such as emergency lighting, fire detection, communications, security, and power distribution. Selecting an appropriate LSZH insulation compound can contribute to safer cable construction when combined with correct installation and system-level fire design.
The broader polyolefin product portfolio of the manufacturer also supports applications in power, communications, locomotives, photovoltaics, new energy generation, marine cables, and rail transit. The specific UV cross-linked B1 or B2 grade should be selected only after confirming the relevant industry standard and finished-cable requirements.
14. Sustainability and Energy-Saving Benefits
The rapid LED UV curing process can contribute to more efficient cable production. A shorter curing stage may reduce line length, shorten production cycles, and lower energy consumption. LED systems can also provide efficient, controllable UV output and may require less operational energy than larger traditional irradiation systems, depending on the equipment configuration and production rate.
Lower equipment investment can make advanced cross-linked LSZH production more accessible to cable manufacturers that cannot justify a large conventional irradiation facility. A more compact process may also reduce the factory space required for curing equipment and simplify plant planning.
Environmental benefits should be evaluated across the complete production and product life cycle. The compound’s LSZH formulation is intended to reduce halogen-related combustion hazards during a fire. Its rapid curing process is intended to reduce manufacturing energy demand. Stable insulation performance may support longer service life and reduce premature replacement. These benefits are most meaningful when supported by accurate process control, responsible material handling, efficient logistics, and appropriate end-of-life management.
Manufacturers should avoid treating energy savings as an automatic result. Actual performance depends on LED efficiency, line speed, cable diameter, UV dose, production utilization, cooling demand, and plant energy management. A plant-level energy assessment can quantify the benefits more accurately for a specific production line.
15. Product Selection and Qualification Considerations
Selection should begin with the project’s fire classification. If a construction project specifies Class B1 or Class B2 performance, the cable manufacturer should determine which grade and finished-cable design can meet that requirement. The compound classification should not be assumed to replace testing of the complete cable assembly.
Operating temperature is another important factor. The DS-ZWG-105 and DS-ZWG-125 designations suggest different temperature-oriented product options, while the B1 and B2 variants are focused on construction fire-performance requirements. The user should confirm the intended continuous operating temperature, emergency overload temperature, and applicable heat-aging criteria in the technical documentation.
Electrical requirements must also be reviewed. Voltage rating, conductor material, insulation thickness, dielectric strength, volume resistivity, capacitance, and insulation resistance may all affect product selection. Communication and data cables may require additional attention to dielectric constant, dissipation factor, impedance, and high-frequency signal behavior, none of which should be inferred solely from the general data listed here.
Processing compatibility should be verified through a production trial. The trial should examine melt stability, surface appearance, insulation concentricity, extrusion pressure, UV dose, line speed, curing level, spark performance, and finished-cable mechanical properties. If the cable includes a sheath or other layers, interlayer adhesion and compatibility should be evaluated as well.
Finally, documentation and supply requirements should be confirmed. Customers may need regular batch consistency, production traceability, technical support, customized colors, special packaging, or delivery arrangements for large projects. A supplier with research, testing, manufacturing, and customization capabilities can help reduce the technical and commercial risks associated with material substitution.
16. Frequently Asked Questions
What is UV Irradiation Cross-linked LSZH Insulation?
It is a low-smoke, zero-halogen cable insulation compound that is extruded onto a conductor and then cross-linked using LED ultraviolet light. The UV exposure activates the curing system and forms a cross-linked polymer structure within a short period.
How quickly does the material cure?
The supplied product information states that cross-linking can be completed within only a few seconds after extrusion. The curing speed is described as dozens of times faster than traditional irradiation cross-linking. Actual speed depends on UV intensity, exposure geometry, line speed, cable size, insulation thickness, and process conditions.
What are the main benefits compared with traditional irradiation cross-linking?
The principal benefits are rapid curing, lower potential equipment investment, reduced energy consumption, shorter production cycles, and easier integration of extrusion and cross-linking. The exact economic benefit depends on the manufacturer’s existing equipment and operating conditions.
Are the B1 and B2 grades suitable for construction cables?
They are designed for construction engineering applications and are intended to meet the combustion performance requirements associated with B1 and B2 classifications under GB 31247-2014. The finished cable should still be tested and approved according to the project specification and applicable certification requirements.
Does the product contain halogens?
The material is an LSZH compound designed to limit halogen-related combustion hazards. The supplied data list HCl and HBr content below 0.5 percent for all four grades. Customers should review the applicable test report and technical documentation for the exact compliance definition used for a specific project.
What smoke-density results are reported?
Under flame conditions, the reported typical smoke-density values are 50, 50, 45, and 40 for DS-ZWG-105, DS-ZWG-125, DS-ZWG-105-B1, and DS-ZWG-105-B2, respectively. Under non-flame conditions, the values are 300, 305, 255, and 265. These are typical values from the supplied product information and should not be treated as a substitute for finished-cable testing.
What mechanical properties are available?
The stated minimum tensile strength is 10.0 MPa and the minimum elongation at break is 150 percent. Typical tensile strength values range from 11 to 13 MPa, while typical elongation at break values range from 160 to 175 percent across the listed grades.
Does the material resist heat deformation?
The supplied data show heat-elongation values of 35 to 45 percent under the listed test conditions, against a stated maximum of 100 percent. Permanent deformation after cooling is listed as zero for all four grades against a stated maximum of 25 percent. The exact test conditions should be confirmed in the current technical documentation.
Can the compound be used on existing extrusion lines?
It may be possible, but compatibility must be verified through a process trial. The extruder, screw, die, cooling system, UV equipment, and line-control system must be suitable for the material. The supplier should be consulted to establish the recommended processing window.
What quality support does the manufacturer provide?
Jiangsu Duoshang New Materials Technology Co., Ltd. states that it provides application-oriented solutions, research and testing support, technical documentation, stable supply capability, and customized material solutions. Its R&D center, production bases, and broad polyolefin product portfolio support project-specific development and qualification.
How should customers choose between the listed grades?
Selection should consider fire classification, operating temperature, mechanical requirements, electrical performance, cable construction, extrusion conditions, and applicable standards. The B1 and B2 grades are focused on construction fire-performance requirements, while the other listed grades may be selected for different temperature or general performance needs. A technical review and trial production are recommended before approval.
17. Conclusion
UV Irradiation Cross-linked LSZH Flame Retardant Insulation for Construction Engineering provides a combination of rapid processing and comprehensive cable performance. Its LED UV curing process is designed to complete cross-linking within seconds, offering a potentially faster, more compact, and more energy-efficient alternative to traditional irradiation cross-linking. This manufacturing advantage is paired with LSZH combustion behavior, low smoke density, low corrosiveness, strong electrical insulation, tensile strength, elongation, and thermal dimensional stability.
The Class B1 and B2 variants are intended for construction engineering applications where flame propagation, heat release, smoke, burning droplets, combustion gases, and corrosiveness must be controlled as part of a broader fire-safety design. The reported performance data show that the listed grades meet the supplied requirements for key mechanical, electrical, thermal, and combustion-related indicators.
Jiangsu Duoshang New Materials Technology Co., Ltd. strengthens the product offering through its R&D infrastructure, research personnel, production capacity, multi-category polyolefin portfolio, and application-oriented support. With more than 3,000 square meters of R&D facilities, more than 10 production lines across two production bases, and experience in multiple cable industries, the company is positioned to support both standardized supply and customized material development.
For cable manufacturers, the most important value is the combination of material capability and process practicality. A compound must not only pass laboratory tests; it must also run consistently on a production line, maintain stable dimensions and insulation quality, support efficient output, and meet the fire and electrical requirements of the final cable. UV cross-linked LSZH technology offers a promising route for achieving that balance in modern construction and infrastructure cable systems.
References
1. GB 31247-2014, Combustion Performance Requirements and Test Methods for Building Materials and Products.
2. Product technical information for UV Irradiation Cross-linked LSZH Flame Retardant Insulation for Construction Engineering, Class B1 and Class B2.
3. Manufacturer-provided main performance data for DS-ZWG-105, DS-ZWG-125, DS-ZWG-105-B1, and DS-ZWG-105-B2.
4. General principles of low-smoke, zero-halogen cable compound formulation and fire-performance evaluation.
5. General principles of ultraviolet curing, polymer cross-linking, and LED UV process control for extruded cable materials.
6. General cable insulation testing practices covering tensile strength, elongation, heat elongation, volume resistivity, dielectric strength, smoke density, acidity, and conductivity.