Content
- 1 Why B1 and B2 LSZH Insulation Materials Matter
- 2 Product Composition and Functional Design
- 3 Manufacturing Process and Quality Control
- 4 Fire Safety Performance
- 5 Mechanical and Thermal Properties
- 6 Electrical Insulation Performance
- 7 Product Grades and Typical Data
- 8 Advantages Compared with Conventional Cable Materials
- 9 Applications
- 10 Manufacturing Strengths of Jiangsu Duoshang New Materials Technology Co., Ltd.
- 11 Research, Testing, and Technical Support
- 12 Recommended Processing Considerations for Cable Manufacturers
- 13 How the Material Supports Sustainable and Safer Cable Design
- 14 Quality and Compliance Considerations
- 15 Frequently Asked Questions
- 15.1 What are B1 and B2 LSZH insulation materials?
- 15.2 What is the difference between the B1 and B2 grades?
- 15.3 Can the compounds be used to claim B1ca, B2ca, or Cca classification automatically?
- 15.4 What is the typical oxygen index?
- 15.5 How do the materials reduce smoke?
- 15.6 Are the materials electrically insulating?
- 15.7 What are the key mechanical properties?
- 15.8 Can the materials withstand elevated temperature?
- 15.9 Are the compounds suitable for cold environments?
- 15.10 What manufacturing technology is used?
- 15.11 What support can a cable manufacturer receive?
- 15.12 Who manufactures these materials?
- 16 Conclusion
- 17 References
- 18 Product: B1 and B2 low smoke halogen-free insulation materials

Modern cable systems must deliver more than electrical conductivity and mechanical durability. In buildings, transportation facilities, data centers, power installations, industrial plants, renewable-energy projects, and public infrastructure, cable materials also play an essential role in fire safety. When a cable is exposed to flame, the insulation and sheath must limit flame spread, reduce smoke generation, avoid the release of corrosive halogen gases, maintain adequate electrical performance, and resist deformation or dripping. These requirements have accelerated the adoption of low-smoke halogen-free, or LSZH, cable compounds.
B1 and B2 low-smoke halogen-free insulation materials are designed for applications requiring a balanced combination of flame retardancy, low smoke emission, reduced corrosiveness, mechanical strength, thermal stability, and electrical insulation. The product described in this article is primarily intended for the insulation layer of BYJ wire. It is formulated from polyolefin resin, high-efficiency compound flame retardants, flame-retardant synergists, carbonization agents, antioxidants, and processing auxiliaries. After controlled mixing, the formulation is pelletized through twin-screw extrusion to create a consistent compound suitable for cable manufacturing.
These materials are developed to satisfy demanding fire-performance classifications, including the B1 and B2 classifications under GB 31247-2014 and the B1ca, B2ca, and Cca classifications under EN 13501-6. The formulation combines a high oxygen index with low smoke density, low halogen-acid generation, low conductivity, and reliable mechanical properties. As a result, it can support cable designs intended for environments where fire safety, low toxicity, and long-term operational reliability are critical.
Why B1 and B2 LSZH Insulation Materials Matter
Traditional halogen-containing cable materials can provide strong flame resistance, but their combustion products may include dense smoke and corrosive gases. In an enclosed environment, smoke can reduce visibility, complicate evacuation, interfere with emergency response, and damage electronic equipment. Acidic gases can also corrode metal components, electrical contacts, control systems, and structural elements.
LSZH compounds are developed to address these concerns. Their formulation avoids the intentional use of halogen-based flame-retardant systems as the primary mechanism for fire protection. Instead, mineral or synergistic flame-retardant systems, carbonization technology, and carefully selected polymer components are used to limit combustion and promote the formation of a protective char or inorganic residue. This approach helps reduce smoke and corrosive emissions while maintaining the physical properties required for cable insulation.
The B1 and B2 grades are particularly relevant when cable installations must meet defined fire-performance levels. The specific classification depends on the complete cable construction, installation conditions, test method, and certification process. The compound itself provides the material foundation for achieving the required cable performance, but the final classification must be verified on the finished cable.
For cable manufacturers, the challenge is not simply to increase flame retardancy. High concentrations of flame retardants can reduce tensile strength, lower elongation, impair processability, increase density, or affect electrical insulation. A successful LSZH compound must balance these competing requirements. It must be flame retardant without becoming excessively brittle, electrically insulating without absorbing unacceptable moisture, and thermally stable without losing dimensional integrity during extrusion or service.
Product Composition and Functional Design
The B1 and B2 insulation materials are based on a polyolefin resin system. Polyolefins are widely used in cable compounds because they offer favorable electrical insulation, chemical resistance, low moisture absorption, and good processing behavior. Their molecular structure can also be modified through formulation and processing to achieve the flexibility and strength required by wire-insulation applications.
The formulation contains several functional groups of ingredients, each serving a specific purpose. The polyolefin resin provides the continuous polymer matrix. It determines the basic flexibility, electrical insulation, melt behavior, and compatibility of the compound. The flame-retardant package helps suppress ignition and flame propagation. Flame-retardant synergists improve the efficiency of the main flame-retardant system, allowing the formulation to achieve the desired performance with a balanced loading level.
Carbonization agents encourage the development of a protective carbonaceous layer or stable residue during combustion. This layer can act as a barrier between the flame and the underlying polymer, limiting heat transfer and reducing the release of combustible decomposition products. Antioxidants protect the polymer during compounding, pelletizing, extrusion, storage, and thermal aging. Processing auxiliaries support dispersion, melt uniformity, surface quality, and stable production.
The effectiveness of an LSZH compound depends not only on the selection of individual ingredients but also on their compatibility and distribution. A flame-retardant system that is poorly dispersed may create weak points, surface defects, unstable electrical properties, or inconsistent fire performance. For this reason, the formulation must be matched with a suitable mixing and extrusion process. Twin-screw compounding provides the intensive mixing, temperature control, residence-time management, and dispersion capability needed for this type of material.
Manufacturing Process and Quality Control
Raw Material Selection
Stable product performance begins with controlled raw material selection. Polyolefin resins must have consistent molecular characteristics and predictable melt behavior. Flame retardants and synergists must meet defined purity, particle-size, moisture, and compatibility requirements. Carbonization agents and antioxidants must be selected according to the expected processing temperature, cable-extrusion conditions, and long-term service environment.
Incoming materials are normally inspected before being released to production. Important control points may include appearance, moisture content, bulk density, particle size, thermal stability, and batch identification. Consistent raw materials reduce variation during compounding and help maintain stable physical and electrical properties between production lots.
Pre-Mixing and Feeding
Before extrusion, the ingredients are proportioned according to the formulation design. Accurate dosing is important because even small variations in the flame-retardant package or antioxidant content can affect oxygen index, smoke generation, tensile properties, and thermal aging results.
Dry blending or pre-mixing helps distribute powdered additives and improves feeding stability. Materials with different bulk densities and flow characteristics must be handled carefully to reduce segregation. Controlled feeding systems can provide a more consistent ingredient ratio throughout the production run. Where required, moisture-sensitive ingredients can be stored and processed under controlled conditions.
Twin-Screw Compounding
The mixed ingredients are processed through a twin-screw extruder. In this equipment, conveying elements transport the materials through multiple processing zones while kneading and mixing elements provide intensive dispersion. The barrel is divided into temperature-controlled sections, allowing the process to be adjusted for melting, wetting, dispersing, homogenizing, and devolatilizing.
Twin-screw technology is particularly suitable for LSZH compounds because the formulation often contains a high level of flame-retardant and mineral components. These additives must be distributed throughout the polymer matrix without excessive shear heating or polymer degradation. The screw configuration can be adapted to promote efficient dispersion while avoiding unnecessary residence time.
Process control includes monitoring melt pressure, melt temperature, screw speed, feeding rate, torque, and throughput. These variables influence the final pellet quality and compound consistency. Excessive temperature may accelerate polymer oxidation or additive degradation. Insufficient mixing may leave agglomerates or create uneven flame-retardant distribution. An optimized process maintains a stable balance between energy input and material throughput.
Pelletizing and Packaging
After compounding, the melt is formed into strands or another suitable shape and pelletized. Pellet size and shape should be consistent so that cable manufacturers can feed the material smoothly into their insulation extruders. Uniform pellets also support accurate blending, storage, transportation, and automatic feeding.
The finished compound is inspected and packed in moisture-resistant packaging suitable for industrial handling. Each batch should be identified with production information that supports traceability. Proper storage helps preserve the material’s processing characteristics and prevents contamination or moisture uptake before use.

B1 and B2 low smoke halogen-free insulation materials
Fire Safety Performance
High Oxygen Index
The oxygen index indicates the minimum oxygen concentration required to support combustion under a specified test method. The reported standard requirement for these materials is at least 28%, while the typical values are approximately 38% to 40% across the listed B1 and B2 grades. This high oxygen index indicates strong resistance to sustained burning under the test conditions.
Ambient air contains approximately 21% oxygen. A material with a higher oxygen index generally requires a more oxygen-rich environment to continue burning. Although oxygen index results do not independently define the complete cable fire classification, they provide a useful indication of the material’s inherent flame-retardant capability.
The typical oxygen-index results demonstrate a performance margin above the stated minimum. The B1 grades show typical values of approximately 40%, while the B2 grades show typical values of approximately 38%. This consistency suggests that the flame-retardant system is designed to provide a stable level of combustion resistance across the product range.
Reduced Smoke Generation
Smoke density is a major consideration for cables installed in occupied or enclosed spaces. The product data lists flaming smoke-density values ranging from approximately 45 to 65, against a stated limit of 100. Under flameless conditions, typical values range from approximately 255 to 275, against a stated limit of 350.
These results indicate that the compounds are designed to limit smoke generation during both flaming and non-flaming exposure. Low smoke performance can help preserve visibility during evacuation and reduce the amount of smoke-related contamination affecting nearby equipment. It is particularly important in transportation systems, tunnels, commercial buildings, hospitals, factories, data centers, and other locations where many people or sensitive systems may be present.
Smoke performance is influenced by the polymer structure, flame-retardant chemistry, carbonization behavior, additive dispersion, and test conditions. Therefore, compound performance should be evaluated together with the finished cable construction. The insulation thickness, conductor type, jacket material, filler system, and cable geometry can all affect the final smoke result.
Low Corrosiveness and Halogen-Acid Control
The HCl and HBr content is listed as less than 0.5% for all typical values. The pH values are approximately 5.1 to 5.2, while conductivity ranges from 0.51 to 0.53 μS/mm. The stated pH requirement is at least 4.3, and the conductivity requirement is no more than 10 μS/mm.
These results indicate low-acid and low-conductivity combustion products under the relevant test procedures. Reducing acid gas and conductivity can help minimize corrosive effects on metal infrastructure and electronic equipment. This characteristic is an important advantage of LSZH materials over conventional halogen-containing systems in sensitive installations.
Low corrosiveness is also relevant to total risk management. A fire can cause extensive damage even after flames have been controlled if acidic smoke attacks control panels, computer equipment, sensors, switchgear, communication systems, or structural metalwork. A low-corrosive cable material helps limit the secondary consequences of fire exposure.
Mechanical and Thermal Properties
Tensile Strength and Elongation
The material has a stated tensile-strength requirement of at least 10.0 MPa. Typical tensile-strength values range from 10 to 11.5 MPa. Elongation at break is specified at no less than 150%, while typical values range from approximately 170% to 180%.
These results indicate that the compound can withstand the mechanical stresses associated with cable manufacturing, installation, bending, pulling, and service. Adequate elongation is particularly important for insulation because cable conductors may experience movement, thermal expansion, vibration, or bending around pulleys and installation routes.
For cable manufacturers, the combination of tensile strength and elongation is more useful than either value alone. A material with high tensile strength but low elongation may be difficult to install and more vulnerable to cracking. A material with very high elongation but insufficient strength may deform excessively during processing or service. The listed results show a balanced mechanical profile suitable for insulation applications.
Thermal Aging Resistance
The air thermal-aging test is conducted at 135°C for 168 hours. The stated change-rate requirement for tensile strength and elongation is within ±25%. The typical tensile-strength changes range from approximately +15% to +18%, while elongation changes range from approximately -13% to -20%.
These results show that the material retains its mechanical integrity after accelerated heat exposure. The increase in tensile strength and decrease in elongation are both within the stated limits. Some post-aging change is expected as polymer chains, additives, and the compound morphology respond to heat. The key consideration is whether the change remains controlled and whether the material retains sufficient strength and flexibility.
Thermal-aging performance supports the use of the compound in cables expected to operate under elevated temperatures or intermittent overload conditions. Actual service temperature depends on the cable design, conductor temperature, installation environment, load profile, and applicable standards. The test results provide an important material-level indication but should not be interpreted as a complete service-life prediction for every cable design.
Hot Elongation and Permanent Deformation
The hot-elongation test is performed at 200°C under a 0.2 MPa load for 15 minutes. The requirement for elongation under load is no more than 100%, and typical results range from approximately 35% to 50%. Permanent deformation after cooling is limited to 25%, while typical results range from -5% to 0%.
Low hot elongation indicates that the insulation can resist excessive stretching when exposed to elevated temperature and mechanical load. This is important because excessive deformation can reduce insulation thickness, affect dimensional stability, and compromise the uniformity of the cable insulation layer.
The low permanent-deformation results indicate that the material largely returns to its original dimensions after the test. Stable recovery helps maintain cable geometry during thermal cycling and reduces the risk of permanent thinning or distortion at elevated temperatures.
Low-Temperature Brittleness
The low-temperature brittleness requirement is listed at -25°C, and all reported typical results are marked as passing. This indicates that the compounds retain sufficient flexibility and resistance to brittle fracture under the specified low-temperature test condition.
Low-temperature performance matters when cables are transported, installed, or operated in cold climates, refrigerated facilities, outdoor infrastructure, railway systems, or seasonal environments. A cable that becomes brittle during cold installation may develop cracks when bent or pulled. Maintaining flexibility at low temperature improves installation reliability and helps preserve insulation integrity over the service life.
Electrical Insulation Performance
Volume Resistivity
The volume resistivity requirement is listed as 1.0 × 1014 Ω·cm at 20°C. Typical values range from approximately 2.3 × 1014 to 5.0 × 1014 Ω·cm. High volume resistivity indicates strong resistance to current flow through the insulation material.
Reliable volume resistivity is essential for preventing leakage current and maintaining circuit separation. It also contributes to stable cable performance in environments where moisture, temperature variation, or electrical stress may affect insulation behavior. The reported typical values provide a significant margin above the stated reference value.
Electrical performance depends on the material formulation as well as the extrusion process. Additive dispersion, moisture control, void prevention, insulation thickness, surface smoothness, and cleanliness can all affect the finished cable’s electrical characteristics. For this reason, compound quality control and cable-extrusion quality control must work together.
Dielectric Strength
The dielectric strength requirement is at least 20 MV/m, while typical values for all listed grades are approximately 28 MV/m. Dielectric strength measures the electric field that the material can withstand before electrical breakdown occurs under specified test conditions.
A high dielectric-strength value supports the use of the compound as an insulating layer in power and control wires. It provides resistance to electrical stress and helps protect against insulation failure when the cable is correctly designed and processed.
To obtain the intended dielectric performance, the cable manufacturer must maintain consistent insulation thickness and avoid contamination, pinholes, voids, and surface damage. The compound provides the necessary material capability, but the final cable result depends on extrusion equipment, tooling, process control, conductor preparation, cooling, and inspection.
Product Grades and Typical Data
The product range includes six identified grades: DS-ZWG-105-B1, DS-WDZF-105-B1, DS-GW-105-B1, DS-ZWG-105-B2, DS-WDZF-105-B2, and DS-GW-105-B2. The following table summarizes the typical values supplied for these grades. The values are representative data and should be confirmed against the applicable technical specification and customer requirements before production approval.
| Property | Unit | Standard or Requirement | DS-ZWG-105-B1 | DS-WDZF-105-B1 | DS-GW-105-B1 | DS-ZWG-105-B2 | DS-WDZF-105-B2 | DS-GW-105-B2 |
|---|---|---|---|---|---|---|---|---|
| Specific Gravity | g/cm³ | Not specified | 1.58 | 1.58 | 1.59 | 1.58 | 1.57 | 1.58 |
| Tensile Strength | MPa | ≥10.0 | 10 | 11 | 11.5 | 10 | 11.5 | 11.5 |
| Elongation at Break | % | ≥150 | 175 | 175 | 170 | 175 | 180 | 175 |
| Oxygen Index | % | ≥28 | 40 | 40 | 40 | 38 | 38 | 38 |
| Hot Elongation at 200°C | % | ≤100 | 35 | 50 | 50 | 35 | 50 | 50 |
| Flaming Smoke Density | — | ≤100 | 45 | 55 | 45 | 45 | 65 | 55 |
| Flameless Smoke Density | — | ≤350 | 255 | 260 | 260 | 255 | 270 | 275 |
| Volume Resistivity at 20°C | Ω·cm | 1.0 × 1014 | 4.5 × 1014 | 5.0 × 1014 | 2.5 × 1014 | 4.5 × 1014 | 4.8 × 1014 | 2.3 × 1014 |
| Dielectric Strength | MV/m | ≥20 | 28 | 28 | 28 | 28 | 28 | 28 |
| pH Value | — | ≥4.3 | 5.2 | 5.1 | 5.1 | 5.2 | 5.2 | 5.2 |
| HCl and HBr Content | % | ≤0.5 | <0.5 | <0.5 | <0.5 | <0.5 | <0.5 | <0.5 |
| Conductivity | μS/mm | ≤10 | 0.51 | 0.53 | 0.53 | 0.51 | 0.51 | 0.52 |
Advantages Compared with Conventional Cable Materials
Lower Smoke and Improved Visibility
One of the main advantages of these LSZH compounds is their focus on smoke reduction. Conventional cable materials may generate dense smoke when exposed to fire, especially in poorly ventilated areas. The reported smoke-density values are substantially below the stated limits for both flaming and flameless conditions. This can support safer evacuation and improve the working conditions of emergency personnel.
Reduced Corrosive Emissions
The low HCl and HBr content, controlled pH, and low conductivity support a reduced-corrosiveness profile. This offers an important advantage in locations containing sensitive electronic systems, communication equipment, control cabinets, precision instruments, and metal infrastructure.
Balanced Mechanical Performance
Some highly filled flame-retardant compounds can suffer from reduced flexibility or poor tensile performance. The listed materials combine a tensile strength of at least 10 MPa with elongation values generally between 170% and 180%. This balance helps the material meet the practical demands of cable processing and installation.
Reliable Thermal Behavior
The compounds demonstrate controlled mechanical changes after aging at 135°C for 168 hours. Their hot-elongation values are significantly below the stated maximum, and permanent deformation after cooling is low. These characteristics distinguish the material from formulations that may soften excessively, stretch under load, or fail to recover after thermal exposure.
Electrical Insulation Capability
High volume resistivity and dielectric strength support dependable electrical insulation. The typical dielectric-strength value of 28 MV/m exceeds the stated minimum of 20 MV/m, while the reported volume-resistivity values are above the listed reference requirement. This provides a strong material basis for reliable cable insulation.
Compliance-Oriented Product Development
The product is developed with reference to B1 and B2 requirements under GB 31247-2014 and B1ca, B2ca, and Cca classification requirements under EN 13501-6. Designing around recognized fire-classification systems gives cable manufacturers a clearer starting point for developing products for domestic and international markets.
It is important to distinguish between compound-level testing and finished-cable certification. The final classification is determined by testing the complete cable in accordance with the applicable standard. Nevertheless, a compound with strong material-level fire, smoke, corrosiveness, mechanical, thermal, and electrical properties can simplify the development path and improve the probability of achieving the targeted cable classification.
Applications
Building and Infrastructure Cables
These materials are suitable for insulation applications in building wires and infrastructure cables where low smoke and low corrosiveness are required. Potential installation environments include commercial buildings, public facilities, high-rise structures, underground spaces, transport hubs, and utility rooms.
Power and Control Wiring
The electrical insulation performance and mechanical balance make the compounds appropriate for selected power, control, and instrumentation cable designs. Designers should confirm conductor size, rated voltage, operating temperature, installation method, and applicable product standard before selecting a specific grade.
Transportation Systems
Railway stations, tunnels, locomotives, metro systems, and other transportation environments place strong emphasis on smoke visibility and fire safety. LSZH insulation materials can contribute to cable systems designed to reduce smoke and corrosive emissions during a fire.
Communication and Data Installations
Communication systems and data centers often contain valuable electronic equipment in enclosed spaces. Low-smoke and low-corrosive cable materials can help reduce secondary damage to equipment and support safer emergency response. The final cable must still meet the relevant electrical, transmission, fire, and installation requirements.
Renewable Energy and New Energy Systems
Photovoltaic installations, energy-storage systems, charging infrastructure, and other new-energy applications require durable and electrically reliable cable materials. Depending on the cable design and environmental exposure, LSZH compounds can be considered where fire safety and reduced smoke are important selection criteria.
Marine and Industrial Cables
Marine facilities, industrial plants, and process-control systems can benefit from low-corrosiveness cable materials, especially where smoke or acidic emissions could affect equipment and personnel. Environmental factors such as oil resistance, water resistance, ultraviolet exposure, flexibility, and temperature must be evaluated separately for each application.
Manufacturing Strengths of Jiangsu Duoshang New Materials Technology Co., Ltd.
Jiangsu Duoshang New Materials Technology Co., Ltd. specializes in the research, development, production, and sale of polyolefin cable compounds. Its focus on polymer-based cable materials enables the company to concentrate resources on formulation design, processing technology, performance testing, and application support.
The company operates a research and development center of more than 3,000 square meters. The center is equipped with more than RMB 35 million worth of research equipment and supported by a professional research team of more than 30 members, including five doctors and several recipients of provincial and municipal talent awards. This research structure supports the development of specialized compounds for different cable constructions and operating environments.
Duoshang operates two production bases covering more than 15,000 square meters, with more than 10 production lines dedicated to polyolefin cable compounds. Multiple production lines can support broader product coverage, production scheduling flexibility, and supply continuity. They also create an infrastructure for manufacturing several compound families while maintaining specialized process conditions for different formulations.
The company’s product portfolio includes eight major categories and more than 50 varieties. These include ultraviolet-crosslinked compounds, silane cross-linkable compounds, irradiation cross-linked compounds, thermoplastic low-smoke halogen-free flame-retardant compounds, polyethylene sheath compounds, and other specialized materials.
This product breadth is valuable to cable manufacturers that require more than one material in their product portfolio. Instead of treating each cable-development project as an isolated purchase, customers can work with a supplier that understands multiple crosslinking systems, sheath technologies, flame-retardant requirements, and cable applications.
Research, Testing, and Technical Support
Advanced material development requires more than formulation ideas. It requires repeatable testing, controlled processing, data interpretation, and practical application support. The company’s R&D resources are intended to support these activities, from initial formulation design through pilot production and customer validation.
Technical documentation can help customers evaluate density, tensile strength, elongation, oxygen index, thermal aging, hot elongation, smoke density, volume resistivity, dielectric strength, low-temperature brittleness, pH, halogen-acid content, and conductivity. These data allow cable engineers to compare material capability with the requirements of their own products.
Application-oriented support is especially important for LSZH compounds because the final performance depends on extrusion conditions. Cable manufacturers may need guidance on drying, feeding, screw configuration, melt temperature, extrusion speed, cooling conditions, die design, conductor preheating, and surface finish. Appropriate recommendations can help reduce startup waste, surface defects, dimensional variation, and insulation-performance failures.
Customized material solutions are also valuable when standard grades do not fully match a customer’s needs. A cable may require a specific balance of flexibility, flame performance, smoke density, thermal resistance, color, processing speed, or electrical properties. Formulation adjustment and controlled validation can help address these requirements while maintaining compliance with the relevant standards.
Recommended Processing Considerations for Cable Manufacturers
Before production, the compound should be stored in clean, dry conditions and protected from contamination. Packaging should remain sealed until the material is ready for use. If the material has been exposed to moisture or unsuitable storage conditions, the manufacturer should evaluate whether drying or additional inspection is necessary.
The extrusion process should be established through controlled trials. Important variables include barrel temperature, die temperature, screw speed, line speed, melt pressure, cooling-water temperature, conductor preheating, and take-up tension. A stable process should produce a smooth insulation surface, consistent diameter, uniform eccentricity, and the required insulation thickness.
Flame-retardant cable compounds may have different flow behavior from unfilled polyolefin materials. The extruder and tooling should therefore be selected and adjusted to accommodate the formulation. Excessive shear or temperature can cause degradation, while inadequate melting or mixing can produce surface roughness and inconsistent properties.
Finished cables should be checked for appearance, dimensions, insulation resistance, voltage withstand, tensile strength, elongation, thermal aging, and any fire-performance requirements specified by the customer or standard. When a cable is intended for B1, B2, B1ca, B2ca, or Cca classification, the complete construction should be tested by an appropriate laboratory under the applicable procedure.
Material selection should also consider the cable’s operating environment. Ultraviolet exposure, oil contact, water immersion, chemical exposure, flexing, vibration, temperature cycling, and installation stress may require additional performance evaluations. The LSZH designation addresses smoke and halogen-related fire behavior, but it does not automatically establish resistance to every environmental condition.
How the Material Supports Sustainable and Safer Cable Design
Low-smoke halogen-free technology supports safer material selection by addressing the consequences of fire in addition to the ability to resist ignition. Reduced smoke can improve visibility, while reduced acid-gas generation can limit corrosion and equipment damage. These benefits are important in the context of total lifecycle risk, particularly for buildings and systems that are expensive or difficult to repair after a fire.
Polyolefin-based compounds can also support efficient cable manufacturing when their processing characteristics are properly controlled. Stable pellet quality, consistent additive dispersion, and repeatable extrusion behavior can help reduce production waste. Long-term cable durability may further reduce replacement frequency, although service life depends on the entire cable design and installation environment.
A responsible approach to material selection should consider the complete product lifecycle. This includes raw material sourcing, energy consumption during compounding and extrusion, product durability, fire performance, maintenance requirements, and end-of-life management. Technical decisions should be based on verified performance data rather than a single environmental claim.
Quality and Compliance Considerations
Customers purchasing B1 and B2 LSZH compounds should request the latest technical data sheet, safety documentation, batch certificate, storage instructions, processing guidance, and applicable test reports. They should also confirm the intended cable application, required classification, rated voltage, conductor type, insulation thickness, and expected operating temperature.
Test results should be interpreted according to the exact method used. Oxygen index, smoke density, pH, conductivity, halogen-acid content, mechanical properties, and dielectric measurements are influenced by specimen preparation and laboratory conditions. Typical values are useful for evaluating normal product performance, but they do not replace acceptance testing or certification of the finished cable.
Traceability is another important quality factor. Batch identification, raw-material records, production parameters, pellet inspection, and final testing provide a foundation for consistent supply. A robust quality system helps identify the cause of deviations and supports corrective action if a customer observes a processing or performance issue.
For international projects, the cable manufacturer should ensure that the selected material and finished cable are evaluated against the standards specified by the project, market, or certification body. GB 31247-2014 and EN 13501-6 address fire classification systems, but other standards may apply to electrical construction, smoke testing, toxicity, halogen content, mechanical behavior, or installation performance.
Frequently Asked Questions
What are B1 and B2 LSZH insulation materials?
They are polyolefin-based cable compounds formulated to provide low smoke generation, low halogen-acid emissions, reduced corrosiveness, flame retardancy, and electrical insulation. They are intended for cable insulation applications such as BYJ wire and related designs.
What is the difference between the B1 and B2 grades?
B1 and B2 refer to different fire-performance levels within the relevant classification systems. The exact classification applies to the finished cable and depends on its complete construction and test results. The supplied compounds provide material options designed for cable manufacturers targeting these levels.
Can the compounds be used to claim B1ca, B2ca, or Cca classification automatically?
No. The compound is designed to support the development of cables targeting these classifications, but the complete cable must be tested under the applicable standard. Insulation, sheath, fillers, conductor arrangement, dimensions, and other construction details affect the final result.
What is the typical oxygen index?
The reported typical oxygen-index values are approximately 40% for the B1 grades and approximately 38% for the B2 grades. The stated requirement is at least 28%.
How do the materials reduce smoke?
The formulation combines a polyolefin resin with a compound flame-retardant system, synergists, carbonization agents, and other auxiliaries. This system is designed to suppress combustion and promote protective residue formation, thereby limiting smoke generation under flaming and flameless conditions.
Are the materials electrically insulating?
Yes. Typical volume resistivity values range from approximately 2.3 × 1014 to 5.0 × 1014 Ω·cm at 20°C, and the typical dielectric strength is approximately 28 MV/m.
What are the key mechanical properties?
The tensile-strength requirement is at least 10.0 MPa, and the elongation-at-break requirement is at least 150%. Typical tensile strength ranges from 10 to 11.5 MPa, while typical elongation ranges from 170% to 180%.
Can the materials withstand elevated temperature?
The materials are evaluated through air thermal aging at 135°C for 168 hours and hot elongation at 200°C under a 0.2 MPa load for 15 minutes. The reported results remain within the stated requirements. Actual cable operating temperature must be determined from the complete cable design.
Are the compounds suitable for cold environments?
All listed grades pass the reported low-temperature brittleness test at -25°C. The final cable should still be evaluated for the specific cold-weather installation and service requirements.
What manufacturing technology is used?
The ingredients are mixed and compounded through twin-screw extrusion before being pelletized. Twin-screw processing supports intensive dispersion, temperature control, and homogeneous distribution of flame-retardant and other functional additives.
What support can a cable manufacturer receive?
Support may include technical documentation, processing guidance, testing assistance, application-oriented recommendations, and customized material development. The exact support should be confirmed according to the customer’s project and technical requirements.
Who manufactures these materials?
Jiangsu Duoshang New Materials Technology Co., Ltd., located in Nantong, Jiangsu Province, China, specializes in polyolefin cable compounds and related polymer materials. The company operates research facilities, production bases, multiple production lines, and a portfolio covering numerous cable-compound categories.
Conclusion
B1 and B2 low-smoke halogen-free insulation materials provide a comprehensive material solution for cable manufacturers seeking strong fire performance without sacrificing electrical and mechanical reliability. Their polyolefin-based formulation combines high oxygen index, controlled smoke density, low halogen-acid content, low conductivity, high volume resistivity, adequate dielectric strength, thermal-aging stability, hot-deformation resistance, and low-temperature flexibility.
The product’s advantages over conventional cable materials are especially relevant in enclosed and high-occupancy environments. Lower smoke generation can support evacuation and emergency response. Reduced corrosive emissions can limit damage to electronic systems and metal infrastructure. Balanced tensile strength and elongation can support cable processing and installation, while stable electrical properties help maintain insulation reliability.
The manufacturing approach is equally important. Controlled raw-material selection, accurate feeding, twin-screw compounding, careful temperature management, consistent pelletizing, and documented quality control help produce a stable compound. Duoshang’s dedicated R&D resources, production bases, specialized polyolefin product portfolio, and application-oriented technical support provide a foundation for serving cable manufacturers in power, communications, transportation, renewable energy, marine, industrial, and building applications.
For the best results, the compound should be selected together with the complete cable design and validated through finished-cable testing. When properly processed and matched to the application, these B1 and B2 LSZH materials can support safer, more reliable, and more compliance-oriented cable systems for demanding domestic and international markets.
References
GB 31247-2014, Classification for Burning Behavior of Electric and Optical Cables.
EN 13501-6, Fire Classification of Construction Products and Building Elements: Classification Using Data from Reaction to Fire Tests on Power, Control and Communication Cables.
Product technical information for B1 and B2 low-smoke halogen-free insulation materials, Jiangsu Duoshang New Materials Technology Co., Ltd.
Technical data concerning oxygen index, smoke density, thermal aging, hot elongation, electrical resistivity, dielectric strength, pH, conductivity, and halogen-acid content supplied for the listed product grades.
General principles of polymer cable-compound formulation, twin-screw compounding, flame-retardant dispersion, and LSZH cable-material processing.

English
Français
Español
русский
عربى